User:Alexander Cvitan/Notebook/Experimental Biological Chemistry Lab/2013/10/23

From OpenWetWare
Jump to navigationJump to search
Biomaterials Design Lab <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

Objective

  • Follow the procedure as outlined by Dr.Hartings HERE.
  • Synthesize more HRP-Linked Au Nanoparticles at higher ratios.
  • Synthesize Myoglobin linked nanoparticles at standard ratios, dictated in yesterdays lab.
  • Run UV-Vis on HRP and Pepsin linked Au-NP's synthesized yesterday.


Procedure

Making HRP and Myoglobin AuNP's

  • In order to synthesize the HRP and Myoglobin nanoparticles, they were made as dictated by the table below.
  • Note that more HRP-Linked nanoparticles are being made because the original ratios made yesterday were large enough to induce fibers to form. We are looking to see at what concentration fibers start forming. Myoglobin nanoparticles are being made at the initial ratios used yesterday.

  • After these solutions were made they were put in then oven at 80 degrees celsius for 4 hours.

UV-Vis of HRP and Pepsin AuNP's

Data