User:Allison K. Alix/Notebook/CHEM-581/2012/09/12
Experimental Chemistry | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
ObjectiveSynthesize polymer film with the addition of gluteraldehyde, exchange clay in solution with a surfactant, synthesize iron oxide DescriptionPROCEDURES: A PVOH (MW=22000, 0.5g, 5ml) film was synthesized using the procedure from 8/29/2012. Before allowing the film to dry, 0.25mL of glutaraldehyde was added with stirring for ~5 minutes. This solution was then left to dry. The clay was exchanged with surfactant in 100 and 50 percents. To create the 100% exchange solution: 2.00 g of clay and 0.7390g of HdMe2Im+ (surfactant) were dissolved in a 50/50 mixture of H2O/ethanol (25mL each) and left to stir for one week. The 50% exchange solution was created with the same parameters except using half the amount of HdMe2Im+ (0.3690g). Data
NotesThis area is for any observations or conclusions that you would like to note.
|