User:Allison K. Alix/Notebook/CHEM-581/2013/02/15
From OpenWetWare
(Difference between revisions)
(→Description) |
(→Description) |
||
| Line 22: | Line 22: | ||
3) 0.14g PVOH, 3mL buffer, 50 mL oil | 3) 0.14g PVOH, 3mL buffer, 50 mL oil | ||
| + | |||
| + | In addition to this, we will cross link already formed hydrogels from [[User:Allison K. Alix/Notebook/CHEM-581/2013/02/01|02/01/2013]] | ||
==Data== | ==Data== | ||
Revision as of 15:21, 18 February 2013
Main project page Previous entry Next entry
| |
|
Objective
DescriptionWe will look at the following solutions for preparing microgels: 1) 0.5g PVOH, 4 mL buffer, 50 mL oil 2) 0.25g PVOH, 3 mL buffer, 50 mL oil 3) 0.14g PVOH, 3mL buffer, 50 mL oil In addition to this, we will cross link already formed hydrogels from 02/01/2013 Data
NotesThis area is for any observations or conclusions that you would like to note.
| |