Part 1: Preparing solutions for coating AuNP with Silica

1) dissolve 0.716g PVP (10kg/mol) in 10mL water (0.00716M)

2) Dissolve 0.42mL NH4OH (29.3wt% NH3 in H2O) in 9.58mL Ethanol (200 proof) (4.2vol%)

NOTE: TES solution will be prepared immediately prior to use to minimize exposure

Part 2: Preparing ZnPPIX solutions