Objectives
ProceduresPart 1: Preparing solutions for coating AuNP with Silica 1) dissolve 0.716g PVP (10kg/mol) in 10mL water (0.00716M) 2) Dissolve 0.42mL NH4OH (29.3wt% NH3 in H2O) in 9.58mL Ethanol (200 proof) (4.2vol%) NOTE: TES solution will be prepared immediately prior to use to minimize exposure
Zinc protoporphyrin (ZnPPIX) samples will be prepared at the same concentrations, following the same procedure as the ThT samples.
V=266.4μL 5μM ZnPPIX in 33.6μL (53.1μ)V=(2.2253μM)(300μL) V=12.57μL DNA in 287.43μL
10% of 250μL=25μL (within 10% allows for accurate concentration comparison) Total solution volume: 275μL (2.068×10-6M)(275×10-6L)=5.31476×10-10moles ZnPPIX (5.31476×10-10moles)/(25×10-6L)=21.3μM ZnPPIX
(5000μM)V=(21.3μM)(25μL) V=0.107μL in 24.9μL
Concentrations: DNA- 0.94μM AuNP- 12.55nM ZnPPIX- 1.9364μM
V=133.2μL ZnPPIX in 166.8μL DataNotes |