User:Allison K. Alix/Notebook/Thesis Research/2013/06/10

From OpenWetWare

(Difference between revisions)
Jump to: navigation, search
(Autocreate 2013/06/10 Entry for User:Allison_K._Alix/Notebook/Thesis_Research)
(Entry title)
Line 6: Line 6:
| colspan="2"|
| colspan="2"|
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
-
==Entry title==
+
==Objectives==
-
* Insert content here...
+
 
 +
* Begin coating AuNP-PVP mixture with silica
 +
 
 +
==Procedures==
 +
 
 +
1) Centrifuge AuNP/PVP solution for 5 minutes at a time at 10,500 rpm 4 times.
 +
 
 +
2) remove supernatant and redisperse with 1mL of 10% NH<sub>3</sub> in ethanol
 +
 
 +
3) Combine redispersions into one container and at 50μL 10% TES in ethanol (5μL TES + 45μL ehtanol)
 +
 
 +
4) Stir for 12 hours

Revision as of 11:13, 10 June 2013

Project name Main project page
Previous entry      Next entry

Objectives

  • Begin coating AuNP-PVP mixture with silica

Procedures

1) Centrifuge AuNP/PVP solution for 5 minutes at a time at 10,500 rpm 4 times.

2) remove supernatant and redisperse with 1mL of 10% NH3 in ethanol

3) Combine redispersions into one container and at 50μL 10% TES in ethanol (5μL TES + 45μL ehtanol)

4) Stir for 12 hours