*Myoglobin stock solution:
*Myoglobin stock solution:
**0.011g x (1 mol/17699g) x 0.010L = 0.0621mM
**0.011g x (1 mol/17699g) x 0.010L = 0.0621mM
-
*Volumes of Au, Myoglobin, and water for each test tube:
+
*Volumes of Au, Myoglobin, and water for each test tube were 5mL
-
**Final [Au]=0.25mM, 5mL total volume
+
[[Image:2014_0129_Au_Myo_NPs_cheat_sheet.PNG|800px]]<br.>
[[Image:2014_0129_Au_Myo_NPs_cheat_sheet.PNG|800px]]<br.>

Current revision

Project name Main project page
Previous entry      Next entry

Method

  • There were a total of 12 gold: nanofiber solutions made, with all of them being the same
  • The ratio of myoglobin to gold was 100:1 and the concentration of gold was 0.25mM
  • Three of the solutions will have the scaffolds in them as this is our first method
  • The other 9 will be used to make the other two methods
  • They were put in an oven for 4hrs at 80°C

Calculations

  • Au stock solution:
    • 0.011g x (1 mol/393.833g) x 0.010L = 2.793mM
  • Myoglobin stock solution:
    • 0.011g x (1 mol/17699g) x 0.010L = 0.0621mM
  • Volumes of Au, Myoglobin, and water for each test tube were 5mL