User:Megan L. Channell/Notebook/Horseradish/2013/09/18: Difference between revisions

From OpenWetWare
Jump to navigationJump to search
(fix raw html notebook nav)
 
(4 intermediate revisions by one other user not shown)
Line 2: Line 2:
|-
|-
|style="background-color: #EEE"|[[Image:BDLlogo_notext_lr.png|128px]]<span style="font-size:22px;"> Biomaterials Design Lab</span>
|style="background-color: #EEE"|[[Image:BDLlogo_notext_lr.png|128px]]<span style="font-size:22px;"> Biomaterials Design Lab</span>
|style="background-color: #F2F2F2" align="center"|<html><img src="/images/9/94/Report.png" border="0" /></html> [[{{#sub:{{FULLPAGENAME}}|0|-11}}|Main project page]]<br />{{#if:{{#lnpreventry:{{FULLPAGENAME}}}}|<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>[[{{#lnpreventry:{{FULLPAGENAME}}}}{{!}}Previous entry]]<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>}}{{#if:{{#lnnextentry:{{FULLPAGENAME}}}}|[[{{#lnnextentry:{{FULLPAGENAME}}}}{{!}}Next entry]]<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>}}
|style="background-color: #F2F2F2" align="center"|[[File:Report.png|frameless|link={{#sub:{{FULLPAGENAME}}|0|-11}}]][[{{#sub:{{FULLPAGENAME}}|0|-11}}|Main project page]]<br />{{#if:{{#lnpreventry:{{FULLPAGENAME}}}}|[[File:Resultset_previous.png|frameless|link={{#lnpreventry:{{FULLPAGENAME}}}}]][[{{#lnpreventry:{{FULLPAGENAME}}}}{{!}}Previous entry]]&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;}}{{#if:{{#lnnextentry:{{FULLPAGENAME}}}}|[[{{#lnnextentry:{{FULLPAGENAME}}}}{{!}}Next entry]][[File:Resultset_next.png|frameless|link={{#lnnextentry:{{FULLPAGENAME}}}}]]}}
|-
|-
| colspan="2"|
| colspan="2"|
Line 14: Line 14:


==Data==
==Data==
The class data follows below:
[[Image:CHEM571_09.18.13_potassiumHRP_Echem_REDOX_table.png]]
[[Image:CHEM571_09.18.13_potassiumHRP_Echem_REDOX_graph.png]]
==Calculations==
*To determine % oxidized, the absorbance peak of 405.32 nm was used from the class data.
*[(Absorbance Value for data pt- Absorbance Min)/(Absorbance Max- Absorbance Min)]*100=% oxidized
* The % Oxidized was subtracted from 100 to calculate the % reduced.


<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->

Latest revision as of 23:23, 26 September 2017

Biomaterials Design Lab Main project page
Previous entry      Next entry

Oxidation and Reduction HRP

Objective

Perform a redox titration on Horseradish Peroxidase to determine the standard potential.

Protocol

The procedure used for the lab comes from Dr. Hartings lab notebook. A total of 5 groups analyzed the cell potential. Group CMJ went first and in the middle of the five runs, the amount of sodium dithionite added to the cell was adjusted. The amounts and concentrations of sodium dithionite added were kept for each group.

Data

The class data follows below:

Calculations

  • To determine % oxidized, the absorbance peak of 405.32 nm was used from the class data.
  • [(Absorbance Value for data pt- Absorbance Min)/(Absorbance Max- Absorbance Min)]*100=% oxidized
  • The % Oxidized was subtracted from 100 to calculate the % reduced.