User:Megan L. Channell/Notebook/Masters Research/2013/10/10: Difference between revisions

From OpenWetWare
Jump to navigationJump to search
No edit summary
Line 7: Line 7:
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit above this line unless you know what you are doing. ##### -->
==PLA Film==
==PLA Film==
* Make PLA film with MOF-5 that was made [[User:Megan L. Channell/Notebook/Masters Research/2013/10/3|this day]]
* Make Polylactic acid (PLA) film with MOF-5 that was made [[User:Megan L. Channell/Notebook/Masters Research/2013/10/3|here]].


==Protocol==
#0.1 %, 0.5 %, 1.0 %, 5.0 %, 10 % and 0 % w/v.


##0.1 % - 0.999 g PLA, 0.001 g MOF-5, 10 mL dichloromethane
##0.5 % - 0.9954 g PLA, 0.0051 g MOF-5, 10 mL dichloromethane
##1.0 % - 0.9902 g PLA, 0.0097 g MOF-5, 10 mL dichloromethane
##5.0 % - 0.9493 g PLA, 0.0497 g MOF-5, 10 mL dichloromethane
##10.0 % - 0.9008 g PLA, 0.0999 g MOF-5, 10 mL dichloromethane
##0 % - 1.0009 g PLA, 10 mL dichloromethane
#Sonicate each sample until dissolved completely.
#Once dissolved, poured into molds to set.
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
|}
|}


__NOTOC__
__NOTOC__

Revision as of 13:39, 10 October 2013

Project name <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

PLA Film

  • Make Polylactic acid (PLA) film with MOF-5 that was made here.

Protocol

  1. 0.1 %, 0.5 %, 1.0 %, 5.0 %, 10 % and 0 % w/v.
    1. 0.1 % - 0.999 g PLA, 0.001 g MOF-5, 10 mL dichloromethane
    2. 0.5 % - 0.9954 g PLA, 0.0051 g MOF-5, 10 mL dichloromethane
    3. 1.0 % - 0.9902 g PLA, 0.0097 g MOF-5, 10 mL dichloromethane
    4. 5.0 % - 0.9493 g PLA, 0.0497 g MOF-5, 10 mL dichloromethane
    5. 10.0 % - 0.9008 g PLA, 0.0999 g MOF-5, 10 mL dichloromethane
    6. 0 % - 1.0009 g PLA, 10 mL dichloromethane
  1. Sonicate each sample until dissolved completely.
  2. Once dissolved, poured into molds to set.