*Made sample with ABS-1.5120g  and MOF-5-.1387g
*Made sample with ABS-1.5120g  and MOF-5-.1387g
*Tested to see how long it takes for color to go through on extruder
*Tested to see how long it takes for color to go through on extruder
 
*[[Image:ABS EXTRUDER 5 16 2014.png]]
*On the XRD above, the plastic was cut into pieces and arranged on the disc. There were some spaces as it is evident on the data.


<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->
<!-- ##### DO NOT edit below this line unless you know what you are doing. ##### -->

Revision as of 11:54, 19 May 2014

Project name <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>

Make filament with MOF-5

  • Extruded filament with MOF-5
  • Made sample with ABS-1.5120g and MOF-5-.1387g
  • Tested to see how long it takes for color to go through on extruder
  • On the XRD above, the plastic was cut into pieces and arranged on the disc. There were some spaces as it is evident on the data.