Creating Thin Polymer Films of PVOH | |||
==Description== | ==Description== |
Revision as of 16:58, 23 September 2012
Experimental Chemistry | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
ObjectiveCreating Thin Polymer Films of PVOH Description1) 22,000 MW PVOH: (a) 0.5 g PVOH was mixed with 3 mL of milli Q water, stirred, and heated to 80 degree Celsius. The solution was placed in a small container up to 48 hrs to allow the thin film formation to occur. (b) 1.01 g of PVOH was mixed with 5 ml of milli Q water and the resulting solution was heated to 80 deg Celsius, until dissolved. The resulting solution was stored for 48 hrs to allow the thin film production to occur. 2) 100, 000 MW PVOH (a) 0.5 g of PVOH was mixed with 5 mL of milliQ water and the resulting solution was heated up to 80 deg Celsius, until dissolved. (b) 1.0 g of PVOH was added in 8 mL of milliQ water and the solution was heated up to 15 mins. Data
NotesThis area is for any observations or conclusions that you would like to note.
|