*Note: Make sure that all glassware is clean and dry. To ensure that the glassware is dry, rinse the glassware with acetone and place in an oven(~60°C) for ~5min to dry. | *Note: Make sure that all glassware is clean and dry. To ensure that the glassware is dry, rinse the glassware with acetone and place in an oven(~60°C) for ~5min to dry. | ||
<br> | <br> | ||
'''CuSO<sub>4</sub> exchanged solutions''' | |||
Revision as of 19:31, 14 October 2012
Project name | <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page <html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html> </html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html> |
Objectives
*NaMT-CuSO4 exchange solution *100% CEC (Bu3HdP+)-MT surfactant clay-CuSO4 exchange solution *50% CEC (Bu3HdP+)-MT surfactant clay-CuSO4 exchange solution
*1.0gPVOH+0.1g NaMT+0.8wt% glutaraldehyde *1.0gPVOH+0.1g 100% CEC (Bu3HdP+)-MT surfactant clay+0.8wt% glutaraldehyde CuSO4 exchanged solutionsGeneral Protocol:
|