Objectives
- Crosslink porphyrin films
- Run AA using film adsorption
- Prepare next highest porphyrin concentration solution. Then add salts to these higher porphyrin solutions
- Run UV-vis on film adsorption and porphyrin-salt solutions
Crosslinking
- The general protocol for porphyrin film crosslinking described on 2012/09/14 was followed for the films listed below
Films Crosslinked:
- PVOH(22K) 1.0073g+1.0mL GA+1mL porphyrin
- PVOH(22K) 1.05225g+1.0mL GA+1mL porphyrin
- For the films listed below, the films were placed in a 6M
|