*After the cross-linking, films became stiffer and their color was not clear as before.
 
*After the cross-linking, film of 100,000 became dark black.
 
*DME results and colors of films!PICTURE!


==Notes==
==Notes==

Revision as of 08:58, 3 October 2012

Experimental Chemistry <html><img src="/images/9/94/Report.png" border="0" /></html> Main project page
<html><img src="/images/c/c3/Resultset_previous.png" border="0" /></html>Previous entry<html>&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;&nbsp;</html>Next entry<html><img src="/images/5/5c/Resultset_next.png" border="0" /></html>


Objective

Description

Part A

  • Dynamic Mechanical Analyzer was used to find out the stiffness and flexibility of each films.(width 5.3 mm)
  • DMA of 22,000 film was measured.(without crosslinking)
  • DMA of 100,000 film wihout cross-linking will be done next week.
  • Following films were cross-linking(kept at 120C for 90min) for DMA.
  • 100,000 PVOH
  • 22,000 PVOH
  • 100,000 PVOH with a drop of HCL
  • 22,000 PVOH with H3Po4 and maleic acid
  • 22,000 PVOH with H3Po4 with H3PO4.

Data

  • After the cross-linking, films became stiffer and their color was not clear as before.
  • After the cross-linking, film of 100,000 became dark black.
  • DME results and colors of films!PICTURE!

Notes

This area is for any observations or conclusions that you would like to note.